Welding a tube film
NOTES ON THE FILM
The film width may not exceed 30 cm. Otherwise it cannot be welded
correctly.
Use only nylon PA/PE films with a structure (dots or grooves) on one side
and a thickness of approx. 0.17–0.29 mm (170–290 μ) in this device.
Otherwise, the weld seam will not be tight and the appliance may be
damaged. You can recognise films of this type from the information on the
packaging. The quality of the weld seam will vary depending on the type
and thickness of the film.
The supplied film is suitable for temperatures between -20°C and +110°C.
The supplied foil is BPA-free and microwaveable. However, never heat
completely sealed bags in the microwave. The bag could burst! One side
of the bag must be open. Heat the bags for no more than 3 minutes at a
maximum temperature of 70°C.
1) Cut the desired length for your bag from the tube film using a pair of scissors.
Cut as straight as possible.
2) Open the appliance lid 1 by pressing the lid release 8 and opening the
lid 1 upwards.
3) Lay the open end of the bag as far into the appliance so that the opening of
the bag is located centrally under the lower sealing ring 5. The bag should
be inserted no further than the rear limiters 6 and must lie between the front
limiters 7. If the bag lies over one or both of the two limiters 6/7, then the
bag cannot be correctly welded.