Harmful chemicals and solvents for rotors
Reduced performance and/or rotor degradation is possible when adsorping the following substances.
Substance
1
Oil vapor
2
Ammonia
3
Amine
4
Hydrogen fluoride
5
Sodium hydroxide
6
Potassium hydrate
7
Lithium chloride
8
Sodium chloride
9
Potassium chloride
10
Calcium chloride
11
Magnesium chloride
12
Aluminum chloride
13
Seawater
14
Strong acid
15
Plasticizer
16
Nitrogen oxides
17
Sulfur oxides
18
High-temperature steam
19
Heat solubility dust
There is no guarantee that other substances beyond this list may reduce the dehumidification performance or damage the silica gel/zeolite.
Compounds-EN v1.1 RevE
Note
2ppm and above, prolonged exposure
High concentration
High concentration
pH=3 and below
High concentration, excessive exposure
High concentration, excessive exposure
Exposod to vapor of 100
and above.
Chemical
formula
N/A
Cloggs the micro pores on the silica gel/zeolite.
NH3
Degrades the silica gel/zeolite.
RNH2
HF
Corrodes the silica gel/zeolite.
NaOH
Dissolves the silica gel/zeolite.
KOH
LiCl
NaCl
KCl
Cloggs the micro pores on the silica gel/zeolite.
CaCl
MgCl
AlCl3
N/A
N/A
Deteriorates the honeycomb's physical structure.
N/A
Cloggs the micro pores on the silica gel/zeolite.
NOx
Deteriorates the honeycomb's physical structure.
SOx
N/A
Cracks occurs on the honyecomb.
N/A
Dust covers the silica gel/zeolite surface.